Symposium on stress-corrosion cracking of metals, held at Philadelphia, Pa., November 29-30 and December 1, 1944, under the joint sponsorship of A. S. T. M. and A. I. M. E
- Författare
- American society for testing materials
- Språk
- Engelska
Förlag | År | Ort | Om boken | ISBN |
---|---|---|---|---|
Pub. jointly by American society for testing materials and Institute of metals division, American institute of mining and metallurgical engineers, New York, N.Y. | 1945 | USA, Philadelphia, Pa | viii, 495 sidor. ill, diagrs 23 cm |